PDF Evaluation of Mount Heaney leads slag to produce a cemented backfill
30 and 60 minute grinds. The puck mill was used to produce 10 and 16 minute grinds. The particle size of these grinds are shown in Figure 3, and are compared to particle size distributions for a typical GP, a typical ground blast furnace slag used by the cement industry, and the lead slag grind used by MICO.